The transition relaxor-paraelectric in Pb(Fe2/3W1/3)O3 ceramics was studied by x-ray diffraction and Raman scattering at temperatures in the range of 85–800 K. For high diffraction angles (160° and 162°), a slight difference between the two phases was found. Raman spectra show an evolution with temperature with anomalies of bands of 848 cm−1 and 147 cm−1 (shift and intensity) in the Curie range of temperatures. This behavior is interpreted as an experimental evidence of perturbations of the nanopolar ordering related to the phase transition.

Evidence of the relaxor-paraelectric phase transition in Pb(Fe2/3W1/3)O3 ceramics

CARNASCIALI, MARIA;NANNI, PAOLO
2002-01-01

Abstract

The transition relaxor-paraelectric in Pb(Fe2/3W1/3)O3 ceramics was studied by x-ray diffraction and Raman scattering at temperatures in the range of 85–800 K. For high diffraction angles (160° and 162°), a slight difference between the two phases was found. Raman spectra show an evolution with temperature with anomalies of bands of 848 cm−1 and 147 cm−1 (shift and intensity) in the Curie range of temperatures. This behavior is interpreted as an experimental evidence of perturbations of the nanopolar ordering related to the phase transition.
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11567/244524
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 33
  • ???jsp.display-item.citation.isi??? 28
social impact